vit-casting-defect / config.json
Zainulabedin1's picture
Initial model upload
de0ce34 verified
Raw History Blame Contribute Delete
1.16 kB
{
"model": "RULLSTM",
"n_features": 17,
"feature_names": [
"op1",
"op2",
"s2",
"s3",
"s4",
"s6",
"s7",
"s8",
"s9",
"s11",
"s12",
"s13",
"s14",
"s15",
"s17",
"s20",
"s21"
],
"hidden": 100,
"layers": 2,
"dropout": 0.5,
"fc": 50,
"window": 30,
"rul_cap": 125,
"normalisation": "minmax",
"norm_lo": [
-0.008700000122189522,
-0.0006000000284984708,
641.2100219726562,
1571.0400390625,
1382.25,
21.600000381469727,
549.8499755859375,
2387.89990234375,
9021.73046875,
46.849998474121094,
518.6900024414062,
2387.8798828125,
8099.93994140625,
8.324899673461914,
388.0,
38.13999938964844,
22.89419937133789
],
"norm_hi": [
0.008700000122189522,
0.0006000000284984708,
644.530029296875,
1616.9100341796875,
1441.489990234375,
21.610000610351562,
556.0599975585938,
2388.56005859375,
9244.58984375,
48.529998779296875,
523.3800048828125,
2388.56005859375,
8293.7197265625,
8.584799766540527,
400.0,
39.43000030517578,
23.61840057373047
]
}